Why Drying PET Before Injection Matters
Residual moisture is the main cause of haze and brittle preforms.
PET is hygroscopic; at melt temperature, water breaks the polymer chains.
Dryer settings
160–170 °C with a 4–6 hour residence time is the most common setup.